Interfacial Fiber Architecture Controls Mode-I Delamination Resistance in
Interfacial fiber orientation plays a decisive role in governing the interlaminar delamination resistance of glass-fiber-reinforced aluminum laminates, outperforming the toughening contributions typically attributed to fiber bridging. In an experimental invest
Illustrative imageInterfacial fiber orientation plays a decisive role in governing the interlaminar delamination resistance of glass-fiber-reinforced aluminum laminates, outperforming the toughening contributions typically attributed to fiber bridging. In an experimental investigation evaluating Mode-I fracture behavior under standardized opening displacement, researchers determined that laminates configured with unidirectional glass fibers aligned perpendicular to the debonding interface achieved propagation fracture toughness values between 1645 and 1720 J/m². This fracture energy significantly exceeded that of interfaces containing fibers aligned parallel to the crack path, which recorded propagation toughness values ranging from 611 to 700 J/m² despite exhibiting substantial mechanical fiber bridging across the advancing crack front.
Fiber–metal laminates, commonly designated as FMLs, integrate thin metallic sheets with fiber-reinforced polymer composite plies to produce hybrid structural materials that combine the ductility, impact performance, and energy absorption of metals with the high strength, fatigue resistance, and low density of composite systems. Among several hybrid formulations developed for structural and aerospace applications, glass-reinforced aluminum laminates, known as GLARE, have seen industrial implementation in primary aircraft components such as Boeing 777 cargo floor panels and Airbus A380 fuselage shells. In these structural assemblies, the hybrid configuration confines fatigue crack growth through intact bridging fibers that span crack faces, decreasing crack opening displacements and lowering effective crack-tip stress intensity factors. However, the integrity and damage tolerance of these laminates depend fundamentally on the metal–composite boundary, where interlaminar delamination remains a primary failure mode capable of degrading laminate stiffness and load-bearing capacity without producing visible external damage.
To evaluate the specific influence of interfacial reinforcement geometry on Mode-I delamination, the investigation prepared and tested four distinct metal–composite interfacial architectures. The experimental design isolated the boundary layer directly adjacent to the aluminum sheet, examining unidirectional plies aligned parallel to the loading direction (AL//0), unidirectional plies aligned transversely at ninety degrees (AL//90), plain-woven fabric plies (AL//PW), and chopped-strand glass-mat configurations (AL//GM). The specimens were fabricated from 0.5-millimeter-thick 6061-T6 aluminum sheets and 400 g/m² E-glass fabrics bonded within an epoxy matrix composed of an LR630 resin and LH630 hardener mixed at a weight ratio of 100:10. To maintain consistent interfacial adhesion across all configurations, the aluminum surfaces underwent uniform preparation consisting of grit-sandblasting to remove contaminants and impart surface roughness, followed by anodization to produce a chemically active oxide layer.
Specimen manufacturing adhered to a vacuum-assisted hand lay-up protocol using an initial resin-to-fiber weight ratio of approximately 1:1 to guarantee full impregnation of the dry glass textiles. The laminates incorporated balanced stacking sequences designed to isolate local interfacial mechanics: the AL//90 configuration followed a sequence designated as [(0/90)₂/0₂/AL//90₂/0₂/AL/0₂], whereas the AL//0 configuration followed [(0/90)₂/0₂/AL//0₂/90/0/AL/(0/90)]. The plain-woven specimens were stacked according to [PW₆/AL//PW₄/AL/PW₂], and the glass-mat specimens were arranged as [0₂/GM₂/0₂/AL//GM₂/0₂/AL/0₂]. Consolidated under vacuum pressure alongside supplementary rigid plates and deadweights to maintain uniform thickness and minimize void formation, the panels were cured at ambient room temperature for 16 hours before receiving an 8-hour post-cure at 60 °C to achieve full resin polymerization.
Double Cantilever Beam testing was conducted in strict accordance with ASTM D5528 standards to evaluate Mode-I critical strain energy release rates and observe real-time crack propagation mechanisms. Individual test specimens were machined to a rectangular geometry measuring 180 millimeters in total length, 25 millimeters in width, and approximately 4.5 millimeters in thickness. An embedded 17-micrometer polytetrafluoroethylene film established a clean 40-millimeter crack-starter front from the loading axis. Symmetrically bonded piano hinges applied tensile opening forces on a universal testing machine operating under displacement control at a constant crosshead speed of 3 millimeters per minute. Crack-front advancement along attached calibrated optical scales was recorded continuously by high-resolution digital cameras, allowing synchronized correlation between instantaneous crack length, applied force, and crosshead displacement.
Data reduction using Modified Beam Theory characterized the compliance calibration and strain energy release rate curves across all interfacial groups. For the AL//90 architecture, the onset of nonlinearity occurred consistently at crack extensions between 11 and 12 millimeters under opening loads spanning 89 to 102 N. The calculated initiation fracture toughness, designated as GIC-Ini, ranged from 977 to 1130 J/m², while steady-state propagation toughness stabilized within a narrow band of 1645 to 1720 J/m². Modified Beam Theory compliance correction factors clustered tightly between 20 and 30, reflecting linear compliance behavior and steady delamination progression with minimal specimen-to-specimen scatter.
Conversely, specimens incorporating the AL//0 interface demonstrated lower fracture resistance despite the emergence of extensive fiber bridging. Under opening displacement, longitudinal glass fibers aligned parallel to crack propagation resisted separation, pulling out from the surrounding epoxy matrix and forming dense bridging ligaments across the opening arms. Notwithstanding this extensive bridging, the measured propagation fracture toughness for the AL//0 interface averaged between 610 and 700 J/m², less than half the toughness recorded for the AL//90 interface. Initiation and propagation toughness curves for AL//0 specimens exhibited noticeable oscillations, which the authors correlated with periodic fiber fracture, bundle pull-out events, and local variations in aluminum surface micro-roughness.
Fractographic analysis resolved the physical mechanisms underlying the superior toughness observed in the AL//90 architecture. Because fibers in the 90-degree plies run perpendicular to the longitudinal tensile opening stress, they do not bridge across the crack faces. Instead, the advancing crack dissipates energy through extensive transverse matrix cracking, local crack deflection, and periodic migration into the adjacent 90°/0° ply boundary. This tortuous crack trajectory was confirmed by post-fracture imaging showing thin residual patches of the 90-degree composite ply adhered to the separated aluminum surfaces. The energy absorbed by multiple microcracking events and crack deflection paths generated an effective fracture resistance that markedly exceeded the energy dissipated by longitudinal fiber bridging in the AL//0 specimens.
Laminates reinforced with plain-woven and chopped-strand glass-mat architectures displayed distinctly heterogeneous fracture responses governed by their respective textile geometries. The AL//PW configuration recorded propagation toughness values between 285 and 338 J/m². The interlacing warp and weft yarns created periodic out-of-plane tow undulations and alternating resin pockets, producing repetitive load drops and serrations in the force–displacement response as the crack alternately encountered resin-rich areas and tightly packed fiber bundles. The chopped-strand AL//GM interface exhibited the widest experimental scatter, with propagation toughness fluctuating broadly between 1100 and 2950 J/m². The irregular, multi-directional distribution of short fibers prevented continuous bridging while generating localized crack arrest and reinitiation sites across resin-rich and fiber-dense regions.
Finite element simulations using cohesive zone modeling implemented in Abaqus evaluated the macroscopic fracture behavior of the experimental specimens without requiring dynamic remeshing. The two-dimensional model discretized the DCB geometry using 5342 four-node plane strain continuum elements (CPE4R) alongside 280 cohesive elements (COH2D4) positioned along the aluminum–composite boundary. The cohesive constitutive formulation employed a bilinear traction–separation law governed by a quadratic nominal stress criterion for damage initiation and an energy-based Benzeggagh–Kenane evolution law for mixed-mode progression. Calibrated cohesive properties, incorporating a penalty stiffness of 5 × 10⁵ N/mm³, an initial normal interfacial strength of 22 N/mm², and an initial shear strength of 40 N/mm², accurately captured the global stiffness, peak load, and post-peak force decay across AL//90, AL//0, and AL//PW interfaces, though the simplified macroscopic formulation did not capture discrete force fluctuations associated with localized bridging and textile undulations.
The study’s scope was bounded by specific experimental conditions, including testing at a single crosshead displacement rate of 3 millimeters per minute under room-temperature laboratory conditions. Fabrications were conducted using vacuum-assisted hand lay-up rather than industrial autoclave processing, and quantitative void-content measurements were not acquired, although identical fabrication, consolidation, and surface preparation protocols ensured fair relative comparisons across all architectures. Additionally, the macroscopic cohesive zone model represented effective interfacial response rather than micro-mechanical damage details. Collectively, the experimental and numerical findings demonstrate that tailoring local interfacial fiber architecture provides a far more potent design strategy for elevating delamination resistance in GLARE structures than relying on fiber bridging alone.
Subject of Research: Interfacial fiber architecture effects on Mode-I delamination in GLARE laminates
Article Title: Influence of Glass Fabric Architecture on Delamination Resistance of GLARE FML
Article References: Mohammadi, B., Mohtasham, A., & Khonsari, M. (2026). Influence of Glass Fabric Architecture on Delamination Resistance of GLARE FML. Applied Composite Materials, 33(4), Article 132. https://doi.org/10.1007/s10443-026-10517-7
Image Credits: AI Generated
DOI: 10.1007/s10443-026-10517-7
Keywords: GLARE, fiber metal laminates, delamination resistance, Mode-I fracture, interfacial architecture, Double Cantilever Beam test, strain energy release rate, fracture toughness, cohesive zone modeling, crack propagation, aluminum epoxy bonding, woven composite, glass mat composite, fiber bridging, ASTM D5528, structural composites
News Source: Scienmag.